MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dymax 9001v3.0 Low Modulus Clear Microencapsulant
Categories: Polymer; Adhesive; Thermoset

Material Notes:
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9001v3.0 Low Modulus Clear Microencapsulant
Lowest stress potting and encapsulation on ceramic, FR-4 or flexible PCBs as well as flip chip, IC cards and other high flow applications Cure Type: UV/Visible Typical Use: High flow for IC cards and flip chip assembly

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 400 cP
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 10.0 sec10-20 mil thick layers cured with Dymax 5000-EC at 2 inches. Thicker layers may require more cure time.
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 310M-2 Optically Clear, Flexible Epoxy
Sika SikaFlex 219 LM Low Modulus Polyurethane Sealant
Dymax 9001v3.1 Resilient, Low Modulus Clear Microencapsulant
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy
Elkem (Bluestar Silicones) BLUESIL™ V 1082 HiPro Clear Silicone Rubber

PDYYMAX51 / 35035

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.