MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik 1201 Synthetic Resin
Categories: Polymer; Thermoset

Material Notes: Synthetic Resin AP is a neutral, unsaponifiable ketone-aldehyde condensation resin. It is generally used in combination with other binders. On account of its wide compatibility and its efficiency, it is used to improve gloss, solids content and covering capacity in the most diverse paint systems.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccSupply form; ISO 758
 1.16 g/cc
@Temperature 20.0 °C
Solid Resin; DIN 53 479-B
Viscosity 1000 cP
@Temperature 23.0 °C
DIN 53 015
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 1.0DIN EN ISO 2114
 
Thermal PropertiesOriginal ValueComments
Softening Point 155 - 170 °CDIN ISO 4625 and DIN 53 181
Glass Transition Temp, Tg 130 °CDIN 53 765
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0DIN ISO 4630
 
Descriptive Properties
Hydroxyl Number (mg KOH/g)200DIN 53 240 mod.
Nonvolatile matter (%)49-51DIN EN ISO 3251

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm DEGALAN® P 28 N Acrylic Resin
Evonik DEGALAN® 4800 L Acrylic Resin
Evonik Compimide® TDAB 2,4-bismaleimidotoluene
Evonik 2220 Adhesion Resin

PHUMB348 / 81350

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.