MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Palm Labs Adhesives Turbo Anti-Seize Nickel Paste
Categories: Metal

Material Notes: TURBO ANTI-SEIZE – NICKEL is a gray, viscous metallic paste which may be used on all bolts, studs, value shafts, value assemblies, transmission shafts, and other types of assembly work where protection against seizing, galling or corrosion is desired. TURBO ANTI-SEIZE – NICKEL will out perform many other anti-seize compounds such as graphite, oil, petroleum, silicone and lead pigments, due to the higher temperature range of this product. It is also slow drying, stays flexible, and withstands pressure to 5000 psi.

Applications:

  • Internal combustion engines: When applied to cylinder head stubs and manifold belts, will prevent seizing. Painted on surfaces such as valve cages, will prevent carbon from fusing to these surfaces.
  • Gaskets: When applied to gaskets, will help maintain the original characteristics of the gasket and will greatly aid in disassembly by allowing the easy removal of the gaskets, saving time on scraping and cleaning.
  • Outboard motors: Can be applied to all studs and cap screws, spark plugs and propeller drive spine shafts, to provide protection against salt water corrosion.
  • Plumbing and Steam Fittings: Will lubricate and protect all joints and gaskets.

Resistance: Water, salt water, gasoline, motor oil, transmission fluid and anti-freeze

Part Numbers for this data: 80-150N

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 7429-90-5, 7440-50-8 and 64742-52-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Viscosity 100000 - 200000 cP100000 - 200000 cP
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 649 °C1200 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Flash Point 177 °C350 °FTOC
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceGray
Uncured stateCastor oil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polykemi AB POLYfill PPH GF5035 PD2 VT Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled/Heat Resistant
Polimersan Plastics POLIPA® (PA 6) Polyamide
Barlog Plastics KEBAFORM C 901 VT POM Copolymer unreinforced, antistatic

PPALML063 / 135217

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.