MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Unirex EP
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Unirex EP 2 is a premium-quality mineral-oil grease. The advanced lithium-complex soap with a combination of an ISO 220 base oil and performance enhancing polymer technology provides excellent high temperature performance, mechanical stability, adhesion, and water resistance. Unirex EP 2 multipurpose grease is highly suitable for a wide range of heavy-duty automotive and industrial applications.

Unirex EP greases are used in a wide variety of sectors including construction, mining, quarrying, cement, logging, pulp and paper-making, and automotive. Specific applications include: Plain and anti-friction bearings in heavy-duty industrial applications; Gear and grid type flexible couplings; Wheel bearings, universal joints, and chassis components

Key Words: NLGI Grade 2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Kinematic Viscosity at 40°C (104°F) 220 cStASTM D445
Oxidative Stability 100 hourPressure Drop of 10 kPa; ASTM D942
 
Mechanical PropertiesOriginal ValueComments
Penetration 8.0Penetration Change, Roll Stability, mm/10; ASTM D1831
 280Worked, 25°C; ASTM D217
Oil Separation 2.0 %ASTM D1742
Timken Test 60.0 lb
 
Thermal PropertiesOriginal ValueComments
Dropping Point 280 °CASTM D2265
 
Descriptive Properties
Colorgreen
Corrosion Prevention, ASTM D1743pass
Soap/Thickener Typelithium complex + polymer
Water Washout, ASTM D1264, wt%3@ 79°C
Wheel Bearing Leakage, ASTM D4290, grams1.4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Unirex N 2
ExxonMobil 2 Mobilith AW Series

WEXXON399 / 75824

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.