System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Manifattura Cattaneo PE HD Polyethylene
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Extruded
Material Notes:
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.
Information provided by Manifattura Cattaneo s.p.a.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.950
g/cc
ISO 1183
Moisture Absorption at Equilibrium
0.010 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation
0.20 %
ISO 62
Mechanical Properties
Original Value
Comments
Hardness, Shore D
66
DIN 53505
Tensile Strength, Yield
23.0
MPa
ISO 527
Elongation at Break
>= 50 %
ISO 527
Elongation at Yield
10 %
ISO 527
Tensile Modulus
1300
MPa
ISO 527
Compressive Yield Strength
9.00
MPa
@Strain 1 %
ISO 604
Poissons Ratio
0.42
Charpy Impact Unnotched
NB
ISO 179
Charpy Impact, Notched
105
kJ/m²
ISO 179
Coefficient of Friction, Dynamic
0.28
on polished steel; MPC Test
Coefficient of Friction, Static
0.18
on polished steel; MPC Test
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+18
ohm-cm
IEC 60093
Surface Resistance
>=
1.00e+13
ohm
IEC 60094
Dielectric Constant
2.4
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength
45.0
kV/mm
@Thickness 2.00 mm
IEC 60243
Dielectric Loss Index
0.00020
@Frequency 1e+6 Hz
IEC 60250
Thermal Properties
Original Value
Comments
CTE, linear
160
µm/m-°C
ASTM D696
Thermal Conductivity
0.400
W/m-K
DOM 52612
Maximum Service Temperature, Air
80.0
°C
Deflection Temperature at 1.8 MPa (264 psi)
44.0
°C
ISO 75
Vicat Softening Point
80.0
°C
ISO 306
Minimum Service Temperature, Air
-100
°C
Flammability, UL94
HB
Compliance Properties
Original Value
Comments
FDA
Yes
Descriptive Properties
Color
Black
Green
White
UV Resistance
N
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Sterigenics Raprex® R100D Branched High Density Polyethylene
Ipiranga Petrochem HC 7260 HDPE
IRPC Polimaxx Polene GA3245 High Density Polyethylene
Isoflon ETFE
Kazanorgsintez PE80B-285SL High Density Polyethylene Composite, Film Grade
PMANIF914 / 156194
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.