MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Akrochem ZDA
Categories: Other Engineering Material

Material Notes: Product Description: AKROCHEM ZDA is a high-quality zinc diacrylate used as a coagent in peroxide cured natural and synthetic elastomers. Zinc diacrylate has found its greatest use in formulations where it contributes to the hardness and high resilience. It can also be used in peroxide cured CSM, CPE NBR, SBR, HNBR, and EPDM compounds where high hardness, high state of cure, and low compression sets are needed. It improves cross-link density of cured products, enhances physical properties such as tensile and tear resistance. Akrochem ZDA also improves rubber to metal adhesion. The finely divided powder form makes the product convenient to weigh and handle.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 - 1.60 g/cc
Particle Mesh Size 80 Mesh100%, no retain
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.30 %
 
Component Elements PropertiesOriginal ValueComments
Zinc, Zn 28 - 32 %
 
Descriptive Properties
AppearanceFree flowing white powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH545 / 315463

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.