MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nabaltec APYRAL® 1E Al(OH)3
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decomposition APYRAL ® does not generate toxic or corrosive gases. In addition, there is a distinct reduction in smoke density. APYRAL ® is effective in the crucial phase of the burning process before the outbreak of a fully developed fire.

APYRAL ® can be used as a flame retardant filler in

  • Thermosets
  • Elastomers
  • Thermoplastics
  • Cable Compounds
  • Technical Rubber Compounds
  • Pressed and cast Plastic Parts
  • Thermal Insulation Foams
  • Glass-fiber reinforced plastics

Key Words: Aluminum Hydroxide, Al(OH)3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.00 g/cc
Density 2.40 g/cc
Brightness 80 %
@Wavelength 457 nm
Whiteness; Elrepho
Oil Absorption 21 %ml/100g
Moisture Absorption at Equilibrium 0.050 %
Loss On Ignition 34.6 %
@Temperature 105 - 1000 °C
Particle Size 50 µmMedian Grain Diameter
Specific Surface Area 0.20 m²/gBET
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 33333 ohm-cm
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.58
 
Component Elements PropertiesOriginal ValueComments
Fe2O3 0.010 %
Na2O 0.20 %
SiO2 0.010 %
 
Descriptive Properties
Al(OH)3 wt %99.7
Crystal StructureGibbsite
Sieve Analysis %50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum Hydroxide, Gibbsite, Al(OH)3
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
EN SPH235 High Manganese Pressure Vessel Carbon Steel
Denka Neoprene W-M1 Polychloroprene Rubber
ASTM A414 Grade A Pressure Vessel Steel, Composition Spec

CNABAL01 / 54526

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.