MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Trinseo BUNA™ SB 1500-SCHKOPAU Cold Polymerised Emulsion Styrene Butadiene Rubber (E-SBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Composition: BUNA™ SB 1500–Schkopau is manufactured by cold polymerization using a rosin acid soap. A discoloring stabilizer is added during the production process.

Application: BUNA™ SB 1500–Schkopau is a general purpose rubber. It can be processed in all sectors of the tire and rubber industry.

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³
Volatiles 0.30 %0.30 %1 hr at 105°C in a hot air oven, 5 g sample; ASTM D5668
Mooney Viscosity 50.2
@Temperature 100 °C
50.2
@Temperature 212 °F
MU, ML 1+4; ASTM D1646
Ash 0.030 %0.030 %ASTM D5667
 
Chemical PropertiesMetricEnglishComments
Styrene Content 23.6 %23.6 %Bound; ASTM D5775
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 27.8 MPa4030 psiCure: 45 min at 145°C; ASTM D412
Elongation at Break 430 %430 %ASTM D412
300% Modulus 18.0 MPa
@Strain 300 %
2610 psi
@Strain 300 %
ASTM D412
 
Descriptive Properties
Organic acid5.7 percentASTM D5774
Rheometer13. mintc(90), ASTM D5289
 2.6 dNmML, ASTM D5289
 21.7 dNmMH, ASTM D5289
 3.9 mints2, 160°C, ASTM D5289
 7.5 mintc(50), ASTM D5289
Test Formulation1 PartStearic acid, ASTM D3185-1A
 1 PartAccelerator (TBBS), ASTM D3185-1A
 1.75 PartsSulfur, ASTM D3185-1A
 100 PartsPolymer, ASTM D3185-1A
 3 PartsZinc oxide, ASTM D3185-1A
 50 PartsCarbon black IRB8, ASTM D3185-1A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Buna® cis 132 High-cis polybutadiene rubber (nickel catalyzed) for tires and rubber articles
Process Technologies Inc BUNA-N Sanitary Gasket

PTRINS9112 / 197582

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.