MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LNP Faradex MS-1002 Polypropylene, Stainless Steel Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Stainless Fiber, EMI

Material Notes:
  • Features: Radio Frequency Shielding, Electromagnetic Shielding, Electrically Conductive
  • Forms: Pellets
  • Processing Method: Injection Molding

Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 15.0 MPaISO 527-1, -2
Tensile Strength, Yield 19.0 MPaISO 527-1, -2
Elongation at Break 70 %ISO 527-1, -2
Elongation at Yield 6.1 %ISO 527-1, -2
Tensile Modulus 1.20 GPaISO 527-1, -2
Flexural Strength 31.0 MPaISO 178
Flexural Modulus 1.40 GPaISO 178
Izod Impact, Notched (ISO) 25.0 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 100 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 10 - 1000 ohmASTM D4496
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1, -2
CTE, linear, Transverse to Flow 160 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °CUnannealed; ISO 75A-1, -2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 232 - 246 °C
Mold Temperature 32.2 - 54.4 °C
Drying Temperature 82.2 °C
Dry Time 4 hour
Back Pressure 0.172 - 0.345 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow DOWSIL™ MS-1002 Optical Grade Moldable Silicone
Avient Stat-Tech™ ST5220-0004 CP4D EG Black Polypropylene Impact Copolymer (PP Impact Copolymer)
LNP Faradex MS-1003 Polypropylene, Stainless Steel Fiber
Hybrid Plastics FireQuench® PM 1287 Resin
Dow HV 1520/50 KIT PARTS A&B

PZLNP1032 / 51114

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.