MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Pro-fax RP735S Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Pro-fax RP735S clarified, easy molding high melt flow polypropylene random copolymer resin is available in pellet form. This resin is typically used in injection molding applications requiring good see-through and contact clarity, along with good impact resistance. Applications: Clear Containers, House wares

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 38 g/10 min
@Load 2.16 kg,
Temperature 230 °C
38 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.9 MPa3900 psi50mm/min; ASTM D638
Elongation at Yield 14 %14 %ASTM D638
Flexural Modulus, 1% Secant 965 MPa140000 psi1.3 in/min, Procedure A; ASTM D790
Izod Impact, Notched 0.690 J/cm
@Temperature 23.0 °C
1.29 ft-lb/in
@Temperature 73.4 °F
Method A; ASTM D256
Gardner Impact 20.3 J15.0 ft-lbASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C165 °Funannealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 11 %
@Thickness 1.14 mm
11 %
@Thickness 0.0450 in
ASTM D1003
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Moplen RP348SK Polypropylene Copolymer
LyondellBasell Pro-fax SV956 Polypropylene Copolymer
LyondellBasell Hifax TYC 1168P NATURAL Polypropylene
ExxonMobil PP7715E4 Impact Copolymer
ExxonMobil PP7035E5 Impact Copolymer

PEQT8806 / 220440

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.