MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

(Viewing data as-entered. Click here to return)
Klinger Thermoseal Klinger® tc-1006 PTFE Gasket Material
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: A high quality, yet cost-effective chemically modified PTFE gasket material that is good to 550°F. A proprietary pressure-sintering and blending process combined with the highest quality raw materials produces a reinforced PTFE sheet that offers superior sealability, excellent torque retention, and reduced creep relaxation. Gaskets cut from this material are suitable for use in strong caustics, moderate acids, chlorine, hydrocarbons, solvents, cryogenics.

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.02 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61ASTM D1700
Tensile Strength 2307 psiASTM F152
Elongation at Break 450 %ASTM D638
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Inert 500 °F
Minimum Service Temperature, Air -350 °F
 
Descriptive Properties
Compressibility3% - 4%ASTM F36
Creep Relaxation0.06ASTM F38
Pressure Limit1200 psi
Recovery0.5ASTM F36
Sealability0.007 ml/hrASTM F37

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röchling Fibracon® PTFE Modified
Fluorseals PTFE Unfilled

PTHERM947 / 192635

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.