MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sibur SKN-26PVC-30 Nitrile-Butadiene Rubber (NBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: For production of rubber and asbestos technical articles which are used as sets for automobile, air planes, different machines and equipment, agricultural, drilling, and polygraph machinery, as well as for production of glues, mastics, and sheaths for cables and shoes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 60 - 80
@Temperature 100 °C
ML 1-4
Ash <= 1.0 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 19.6 MPa
Elongation at Break >= 450 %
 
Descriptive Properties
Loss During Drying<1%
Mass Share of Combined Nitrile and Acrylic Acid28-32%
Mass Share of Ionol>0.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nitriflex N-206 NBR - Nitrile Rubber
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Precision Polymer Engineering N70C Nitrile Rubber
Process Technologies Inc BUNA-N/Metal - Metal Detectable Sanitary Gasket
Dow Buna® SB 1721 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR)

PSIB122 / 67685

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.