MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Ateva® 2803A Ethylene Vinyl Acetate Copolymer Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade

Material Notes: Designed for extrusion and injection molding applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/ccASTM D1505, ASTM D1928 Proc A
Vinyl Acetate Content 28 %
Melt Flow 3.0 g/10 minASTM D1238 190/2.16
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 84ASTM D2240
Hardness, Shore D 30ASTM D2240
Tensile Strength, Ultimate 17.0 MPaASTM D638 Type IV
Elongation at Break 770 %ASTM D638 Type IV
Flexural Yield Strength 17.0 MPa1% secant, ASTM D790 Method I
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 44.0 °CASTM D1525
Brittleness Temperature <= -85.0 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Ateva® 2803G Ethylene Vinyl Acetate Copolymer
Celanese Ateva® 1241 EVA polymer for compounds, flexible packaging and foam
Celanese Ateva® 1821 Ethylene Vinyl Acetate Copolymer Film
Celanese Ateva® 1825A Ethylene Vinyl Acetate Copolymer Film
Celanese Ateva® 1641 Ethylene Vinyl Acetate Copolymer Coating Resin

PATEVA33 / 25950

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.