MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Selenis BONDZ GG 174 Copolyester for Coextruded Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP

Material Notes: Selenis Bondz GG 174 is a copolyester specifically designed for sealing layers in GAG coextruded films. Selenis has developed this bonding solution to consistently deliver excellent melt strength and exceptional heat-sealing performance. This product is formulated to provide and sustain the adhesion level crucial to the packaging integrity through the different processes of manufacturing, from coextrusion to thermoforming, securing full protection of the final product. Selenis Bondz GG 174 greatly improves film, providing enhanced printability, effortless trimming and easier thermoformability; hence boosting energy efficiency. Selenis Bondz GG 174 may be used as a primary or secondary packaging material for thermoformed trays, blister applications, and form-fill-seal applications up to 75ºC. Selenis Bondz GG 174 guarantees no crystalline haze; thereby assuring film will be crystal-clear. This solution ensures exceptional adhesion level, while maintaining high clarity and gloss, certifying optimal visual appeal at point of sale.

Information provided by Selenis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.730 g/cc
Density 1.27 g/ccASTM D792
Moisture Absorption at Equilibrium <= 0.30 %
Viscosity Test 72 - 76 cm³/gIntrinsic; ISO 1628-5
ASTM Color <= 1.0b*; ASTM D6290
 >= 64L*; ASTM D6290
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 85.0 °CASTM D3418
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 250 °C
Drying Temperature <= 70.0 °Cto avoid chips sticking together in dryer hopper
 60.0 - 65.0 °C
@Time 21600 - 28800 sec
Moisture Content <= 0.0040 %dried
Dew Point -40.0 °C
 
Descriptive Properties
Food Approval PharmacopeiaYes
Particle size320 ± 50 mg/20 chips
Pellet ShapeCylindrical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSELE923 / 243421

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.