MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Celanese Celstran® PPS-GF50-01-US PPS, 50% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler

Material Notes: 50% long strand glass fiber reinforced polyphenylene sulfide
50% long strand glass fiber reinforced polyphenylene sulfide. UL-V0 flame retardant.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.72 g/ccASTM D792
Density 1.72 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0040 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 150 MPa5mm/min; ISO 527-2/1A
 25600 psiASTM D638
 26100 psi
@Temperature -40.0 °C
ASTM D638
Elongation at Break 1.04 %5mm/min; ISO 527-2/1A
 0.95 %
@Temperature -40.0 °C
ASTM D638
 1.0 %
@Temperature 22.8 °C
ASTM D638
Tensile Modulus 18200 MPa1mm/min; ISO 527-2/1A
 2.93e+6 psi
@Temperature 22.8 °C
ASTM D638
 3.11e+6 psi
@Temperature -40.0 °C
ASTM D638
Flexural Strength 265 MPaISO 178
 38400 psiASTM D790
 39100 psi
@Temperature -40.0 °C
ASTM D790
Flexural Modulus 17300 MPaISO 178
 2.51e+6 psi
@Temperature 22.8 °C
ASTM D790
 2.71e+6 psi
@Temperature -40.0 °C
ASTM D790
Izod Impact, Notched 6.90 ft-lb/inASTM D256
 7.00 ft-lb/in
@Temperature -40.0 °C
ASTM D256
Charpy Impact, Notched 23.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 282 °CISO 75-1, -2
 540 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 - 80.0 °C
 140 - 160 °CCavity temperature
Feed Temperature 20.0 - 50.0 °C
Zone 1 285 - 295 °C
Zone 2 290 - 300 °C
Zone 3 295 - 305 °C
Zone 4 300 - 310 °C
Die Temperature 290 - 300 °C
Melt Temperature 300 - 310 °C
Drying Temperature 130 - 140 °C
Dry Time 3.00 - 4.00 hour
Moisture Content 0.020 %Necessary low maximum residual
Dew Point <= -30.0 °CPre-drying
 
Descriptive Properties
Longer pre-drying times/storagelower the temperature to 100° C until processed.<= 60 h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayblend® T88 GF-20 Polycarbonate + SAN Glass Filled Impact Grade
Celanese Celstran® PP-GF50-03 PP, 50% Glass Reinforced
Celanese Celstran® PP-GF50-0455P10/10 PP, 50% Glass Reinforced
Celanese Celstran® PP-GF50-0458 P10/10 PP, 50% Glass Reinforced
Celanese Celstran® PP-GF50-BV337 PP, 50% Glass Reinforced

PHCR226 / 158795

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.