MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PSC 500 Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Polystyrene 500 is a high melt, easy flow crystal polystyrene for fast cycle injection molding. The high flow characteristics of this material make it easy to fill thin parts.

500 is utilized in products such as cutlery, tumblers, and containers. Other features are excellent clarity and FDA compliance.

Information provided by Total Petrochemicals, Inc.

Key Words: High melt, easy flow, crystal
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 14 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 6100 psiASTM D638
Tensile Modulus 420000 psiASTM D638
Flexural Strength 11000 psiASTM D790
Flexural Modulus 440 ksiASTM D790
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 188 °FHeat Distortion, Annealed; ASTM D648
Vicat Softening Point 200 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PSC 585 Polystyrene
Total PSC 1540(AS) Crystal Polystyrene
Total PSC 536 Polystyrene
Total PSC 1540(EU) Crystal Polystyrene
Total PSC 535 Polystyrene

PFIM900 / 38305

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.