#71 Styrene Wax is a 5% solution of paraffin dissolved in styrene that may be added to non waxed polyester resins and gel coats to prevent the prolonged tackiness associated with thin sections of polyesters. If the resin contains paraffins, the wax will rise to the surface and protect the curing resin from the inhibiting action of the air. However, if the resin is allowed to fully cure, the paraffins on the surface will prevent adhesion of further coats of resin and must be sanded off prior to additional applications. Fibre Glast recommends adding #71 at 5% for thin coatings. Use with #1040 Hi-Gloss Additive when performing repairs below the water line. |