MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :
  • electrical conductivity greatly superior to that of bronzes, brasses and nickel silver
  • mechanicals properties on a par with those of copper cobalt- beryllium and of bronze
  • excellent fatigue strength
  • very competitive cost compared with copper-cobalt-beryllium.

Information provided by CLAL-MSX

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 105 - 125105 - 125
 194
@Time 3600 sec
194
@Time 1.00 hour
 200
@Time 7200 sec
200
@Time 2.00 hour
 200
@Time 18000 sec
200
@Time 5.00 hour
 203
@Time 14400 sec
203
@Time 4.00 hour
 205
@Time 10800 sec
205
@Time 3.00 hour
Tensile Strength, Ultimate 320 - 400 MPa46400 - 58000 psi
Tensile Strength, Yield 290 - 380 MPa
@Strain 0.2 %
42100 - 55100 psi
@Strain 0.2 %
Elongation at Break 10 - 20 %10 - 20 %
Fatigue Strength 245 MPa
@# of Cycles 1.00e+7
35500 psi
@# of Cycles 1.00e+7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.00000400 ohm-cm<= 0.00000400 ohm-cmprecipitation hardened
 0.00000420 ohm-cm0.00000420 ohm-cmprecipitation hardened (2 hr)
 0.00000420 ohm-cm0.00000420 ohm-cmprecipitation hardened (3 hr)
 0.00000420 ohm-cm0.00000420 ohm-cmprecipitation hardened (4 hr)
 0.00000430 ohm-cm0.00000430 ohm-cmprecipitation hardened (5 hr)
 0.00000430 ohm-cm0.00000430 ohm-cmprecipitation hardened (1 hr)
 0.00000780 ohm-cm0.00000780 ohm-cmquenched
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.0 µm/m-°C
@Temperature 20.0 - 300 °C
10.6 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.370 J/g-°C0.0884 BTU/lb-°F
Thermal Conductivity 84.0 W/m-K583 BTU-in/hr-ft²-°Fsolid solution (or quenched) state
 188.4 W/m-K1307 BTU-in/hr-ft²-°Fquenched state
Melting Point 1040 - 1060 °C1900 - 1940 °F
Solidus 1040 °C1900 °F
Liquidus 1060 °C1940 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 96.9 %96.9 %
Nickel, Ni 2.5 %2.5 %
Silicon, Si 0.60 %0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion Beryllium Copper Alloy 190 Strip; 1/2HM (TM02) Temper (UNS C17200)
CLAL-MSX NICLAFOR® 1000 TDX Quenched/Cold Rolled, Drawn Copper Alloy
Beryllium Copper, UNS C17200, TM08 Temper Strip
Beryllium Copper, UNS C17200, TM06 Temper Strip

NCLAL094 / 160125

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.