MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Avient Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Polyphenylene Sulfide (PPS)

Material Notes: Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low to high levels of conductivity depending upon application requirements.

Information provided by PolyOne

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.014 - 0.015 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 81.4 MPaASTM D638
Elongation at Break 0.75 %Type I, 5.1 mm/min; ASTM D638
Flexural Strength 116 MPaASTM D790
Flexural Modulus 12400 MPaASTM D790
Izod Impact, Notched 22.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10 - 1000 ohm-cmASTM D257
Surface Resistance 100 - 10000 ohmASTM D257
Static Decay 0.0020 sec(Mil-B-81705C), 12% RH, 5000kV to 50kV
Shielding Effectiveness 40 dB
@Frequency 1e+9 Hz
1/8 thickness
 55 dB
@Frequency 5.00e+9 Hz
1/8 thickness
 61 dB
@Frequency 1e+10 Hz
1/8 thickness
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) >= 245 °CUnannealed; ASTM D648
 
Descriptive Properties
FeaturesElectromagnetic Shielding (EMI)
Filler / ReinforcementNickel-Coated Carbon Fiber
FormsPellets
Generic MaterialLCP+PPS
Generic NameLiquid Crystal Polymer + PPS (LCP+PPS)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAerospace Applications
 Automotive Electronics
 Computer Components
 Connectors
 Electrical Housing
 Electrical/Electronic Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese VECTRA A950 LCP, Unfilled
Celanese VECTRA E488i LCP, Specialty
Celanese VECTRAN™ V300P Co-Extrudable Liquid Crystal Polymer (LCP)
Avient Stat-Tech™ LC-40CF/000 Natural LCP (Liquid Crystal Polymer), 40% Carbon Fiber Reinforced, Electrically Conductive, EMI/RFI Shielding
Avient Stat-Tech™ LC-20NCF/000 V3 RD 4020 Liquid Crystal Polymer (LCP)

PH0POL1343 / 145912

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.