MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Poco Graphite SUPERSiC® Si-8C Silicon Carbide
Categories: Ceramic; Carbide

Material Notes: SUPERSiC that has been infiltrated with silicon and then coated with a 200 µm CVD SiC coating

Uses: Ideal for optical and lithography components

Information provided by Poco Graphite

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.95 g/cc
Density 3.03 g/cc
Porosity 0.00 %porosity sealed off by CVD SiC coating
 4.0 %porosity is sealed under the dense coating, porosity is not exposed to the process
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 17940 psi
Modulus of Elasticity 338 GPa
Flexural Strength 32360 psi
Poissons Ratio 0.17
Fracture Toughness 2.63 MPa-m½
Shear Modulus 138 GPaDynamic
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00400 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.40 µm/m-°C
Thermal Conductivity 220 W/m-K
 
Descriptive Properties
Specific stiffness121 kN.m/g
Total impurity level<10 ppm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NeoGraf eGRAF® HITHERM™ HT-1220 Graphite
Poco Graphite SUPERSiC® Basic Silicon Carbide
Poco Graphite SUPERSiC® 3CX Silicon Carbide
Poco Graphite SUPERSiC® Si Silicon Carbide
Ceradyne CeraTrex™ 146-3E Silicon Carbide

CPOCO44 / 133184

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.