MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion Copper Beryllium Alloy 165 Cold Rolled (Heat Treatable) Strip ¼ H (TD01) (UNS C72900)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Alloy 165 strip provides strength and conductivity close to Alloy 25 strip, with slightly less beryllium. Since it is heat treated after forming, it provides excellent formability and ductility. This alloy features good stress relaxation resistance and high fatigue strength. Typical applications include pressure sensor bellows, burn-in and test socket contacts, computer processor socket contacts, and electromagnetic shielding gaskets.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.41 g/cc0.304 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 121 - 185121 - 185DPH Hardness
Tensile Strength, Ultimate 517 - 607 MPa75000 - 88000 psi
Tensile Strength, Yield 414 - 552 MPa
@Strain 0.200 %
60000 - 80000 psi
@Strain 0.200 %
Elongation at Break 15.0 - 45.0 %15.0 - 45.0 %
Modulus of Elasticity 131 GPa19000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000610 - 0.00000780 ohm-cm0.00000610 - 0.00000780 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.5 µm/m-°C9.70 µin/in-°F
Thermal Conductivity 105 W/m-K729 BTU-in/hr-ft²-°F
Melting Point 870 °C1600 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 1.60 - 1.85 %1.60 - 1.85 %
Co + Ni >= 0.200 %>= 0.200 %
Co + Ni + Fe <= 0.600 %<= 0.600 %
Copper, Cu 97.55 - 98.2 %97.55 - 98.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBB442ub / 323461

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.