MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grivory® TR90 Transparent Nylon 12, As Conditioned  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Grilamid TR 90 is a transparent polyamide with good heat resistance and excellent fatigue behavior. Grilamid TR 90 also exhibits low moisture absorption and dimensional stability.

Grilamid TR 90 was developed for use in filter bowls, eye glass frames, tooth brushes and optical fiber containing cables. It may also be considered for a variety of consumer and industrial applications in which chemical resistance, transparency and toughness are desired.

Because Grilamid TR 90 contains no plasticizer and resists cosmetic chemicals and perspiration, it can enhance the design and performance of personal products such as sport and safety spectacle frames. Grilamid TR 90 is NSF Standard 61 Listed.

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ASTM D792
Water Absorption 0.40 %0.40 %24 hr immersion; ASTM D570
Moisture Absorption at Equilibrium 1.5 %1.5 %23°C / 50% RH; ASTM D570
Water Absorption at Saturation 3.3 %3.3 %23°C in water; ASTM D570
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8484
Tensile Strength at Break 57.0 MPa8270 psiASTM D638
Elongation at Break 150 %150 %ASTM D638
Elongation at Yield 10 %10 %ASTM D638
Flexural Strength 82.0 MPa11900 psiASTM D790
Flexural Modulus 1.58 GPa229 ksiASTM D790
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmDIN 53481
Dielectric Constant 2.8
@Frequency 100 Hz
2.8
@Frequency 100 Hz
IEC 250
Dielectric Strength 34.0 kV/mm864 kV/inDIN 53481
Dissipation Factor 0.0011
@Frequency 100 Hz
0.0011
@Frequency 100 Hz
IEC 250
Comparative Tracking Index >= 600 V>= 600 VDIN 53480
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 °C
5.00 µin/in-°F
@Temperature 68.0 °F
DIN 53752
Specific Heat Capacity 1.80 J/g-°C0.430 BTU/lb-°FEMS
Thermal Conductivity 0.160 W/m-K1.11 BTU-in/hr-ft²-°FEMS
Maximum Service Temperature, Air 80.0 °C176 °FLong Term; EMS
 100 °C212 °FShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 127 °C261 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 113 °C235 °FASTM D648
Glass Transition Temp, Tg 155 °C311 °FDSC
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.511.51DIN 53491
Transmission, Visible 92 %92 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FClamp (Extrusion)
Rear Barrel Temperature 260 °C500 °FExtrusion
Middle Barrel Temperature 260 °C500 °FExtrusion
Front Barrel Temperature 250 °C482 °FExtrusion
Die Temperature 260 °C500 °FExtrusion
Melt Temperature 270 - 280 °C518 - 536 °FInjection molding
Mold Temperature 80.0 °C176 °FInjection molding

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
301 Stainless Steel
EMS-Grivory Grilamid® LV-15H nat PA12-GF15
Alclad Aluminum 6061-T6, T651
Multibase TPSiV® 4000-70A Thermoplastic Silicone Vulcanizate
Alliance N-42H Neodymium Iron Boron Magnetic Material

PGRIK131 / 42601

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.