MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese HQ 68-50001461 Vinyl Acetate
Categories: Fluid

Material Notes: CAS Number: 108-05-4

Vinyl Acetate is a clear, colorless liquid with a faint ether-like odor. It is only sparingly soluble in water but readily soluble in many organic solvents such as ethyl acetate and ethanol. It is a highly flammable liquid. In the presence of water, it forms an azeotrope, which boils at 66 °C under atmospheric pressure, that contains 92.7 % Vinyl Acetate. Vinyl Acetate is stabilized with 3 – 5 ppm of Hydroquinone to prevent uncontrolled polymerization during handling and storage. Vinyl Acetate with higher amount of hydroquinone is available upon request.

Applications: reactions with other esters. This chemical property makes it a very versatile monomer; it readily forms homo-polymers and hetero-polymers with a wide range of other monomers such as ethylene, acrylates, vinyl chloride, fumarate esters, and maleate esters among others. It polymerizes under the influence of various activators such as light, heat or peroxides. The vinyl acetate monomer can be polymerized in the mass as well as in the form of a solution, suspension (pearl form) or emulsion. The latter form is widely used for the production of synthetic resin dispersions, general and pressure sensitive adhesives and in the paint, textile and paper coating industries. Solution and suspension polymers are used in coatings and adhesives. Suspension polymers, in addition, are used in plastics. Secondary products from vinyl acetate polymers are the polyvinyl alcohols, from which the polyvinyl acetals are produced. Fields of applications for polyvinyl acetate, polyvinyl acetate secondary products and their co- and terpolymers are:
Polyvinyl acetate is suitable as a binder and raw material for the production of paints, adhesives, paper coatings, finishing agents for textiles and non-wovens, and resin-bound plasters.
Polyvinyl alcohol is employed as a thickening agent and protective colloid and is also used in the form of a solution, for instance in the production of adhesives, paper, textiles and cosmetics.
Polyvinyl acetals, e.g. polyvinyl butyral, are used for instance in the manufacture of paints, primers, electrical resins, printing inks and films for laminated glass.
Acrylonitrile / vinyl acetate copolymers are employed in the production of acrylic fibers.
Methacrylic acid / vinyl acetate copolymers are suitable for the production of paints for interior and exterior use. Vinyl acetate/ethylene/vinylchloride (VAEVC) terpolymers are used in the form of dispersions for the production of abrasion-resistant interior paints, exterior wall paints, resin-bound plasters and cement additives.
Vinyl acetate/ethylene (VAE) and vinyl acetate/vinyl versatate copolymers with a predominance of Vinyl acetate are employed as dispersions e.g. for the production of adhesive films for textiles (nonwovens) and crosslinking agents.
Ethylene/Vinyl acetate (EVA) copolymers with a large proportion of ethylene are suitable for the modification of low-density polyethylene for engineering plastics (e.g. automotive industry) and for the production of shrink film and other films.
Ethylene / vinyl alcohol (EVOH) copolymers are used for the production of food packaging materials because of their excellent oxygen barrier properties.

Information provided by Celanese Corporation.

Key Words: VAM; acetic acid vinyl ester; acetic acid ethenyl ester; ethenyl acetate; ethenyl ethanoate; vinyl acetate monomer; 1-acetoxyethylene; VA; C4H6O2; C4H6O2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.00366 g/ccVapor density
 0.8947 g/cc
@Temperature 50.0 °C
 0.9011 g/cc
@Temperature 45.0 °C
 0.9075 g/cc
@Temperature 40.0 °C
 0.9138 g/cc
@Temperature 35.0 °C
 0.920 g/cc
@Temperature 30.0 °C
 0.9262 g/cc
@Temperature 25.0 °C
 0.9323 g/cc
@Temperature 20.0 °C
 0.93984 g/cc
@Temperature 15.0 °C
 0.9444 g/cc
@Temperature 10.0 °C
 0.9503 g/cc
@Temperature 5.00 °C
 0.9562 g/cc
@Temperature 0.000 °C
Solubility in Water 2.3 %
Viscosity 0.32 cP
@Temperature 50.0 °C
 0.38 cP
@Temperature 30.0 °C
 0.43 cP
@Temperature 20.0 °C
Molecular Weight 86.09 g/mol
Vapor Pressure 0.0407 bar
@Temperature 0.000 °C
 0.0540 bar
@Temperature 5.00 °C
 0.0710 bar
@Temperature 10.0 °C
 0.0923 bar
@Temperature 15.0 °C
 0.1187 bar
@Temperature 20.0 °C
 0.15152 bar
@Temperature 25.0 °C
 0.1908 bar
@Temperature 30.0 °C
 0.2386 bar
@Temperature 35.0 °C
 0.296 bar
@Temperature 40.0 °C
 0.3643 bar
@Temperature 45.0 °C
 0.4449 bar
@Temperature 50.0 °C
Surface Tension 19.8 dynes/cm
@Temperature 50.0 °C
 22.3 dynes/cm
@Temperature 30.0 °C
 23.6 dynes/cm
@Temperature 20.0 °C
Storage Temperature <= 30.0 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 385 J/g
@Temperature 50.0 °C
 399 J/g
@Temperature 30.0 °C
 406 J/g
@Temperature 20.0 °C
Specific Heat Capacity 1.97 J/g-°C
@Temperature 20.0 °C
 2.01 J/g-°C
@Temperature 30.0 °C
 2.10 J/g-°C
@Temperature 50.0 °C
Thermal Conductivity 0.141 W/m-K
@Temperature 50.0 °C
 0.149 W/m-K
@Temperature 30.0 °C
 0.152 W/m-K
@Temperature 20.0 °C
Melting Point -92.8 °C
Boiling Point 72.7 °C
@Pressure 0.101 MPa
Flash Point -8.00 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.395
@Temperature 20.0 °C
nD
 
Processing PropertiesOriginal ValueComments
Shelf Life 2.00 MonthBulk
 6.00 MonthDrums 3-5 ppm HQ
 12.0 MonthDrums 14-17 ppm HQ
 
Descriptive Properties
Water Solubility1% Water in Vinyl Acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese HQ 812-50001463 Vinyl Acetate
3M K37 Glass Bubbles
3M S38HS Glass Bubbles
3M S38 Glass Bubbles
Celanese 50000445 Methyl Isobutyl Carbinol (MIBC)

WCELAN960 / 178031

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.