MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound KX06415 Acetal (POM) Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: LNP LUBRICOMP KX06415 compound is based on Acetal (POM) Copolymer resin containing 10% PTFE, 10% aramid powder. Added features of this grade include: Easy Molding, Heat Stabilized, Wear Resistant.

Features: Wear resistant,Heat Stabilized,Easy Molding

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Density 1.45 g/ccASTM D792
Moisture Absorption 0.210 %23°C/50% RH/24 hrs; ASTM D570
 0.350 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.020 - 0.040 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 39.0 MPa5 mm/min; ISO 527
 41.0 MPa5 mm/min; ASTM D638
Elongation at Break 14 %5 mm/min; ASTM D638
 14 %5 mm/min; ISO 527
Elongation at Yield 8.5 %5 mm/min; ASTM D638
 8.8 %5 mm/min; ISO 527
Tensile Modulus 2590 MPa1 mm/min; ISO 527
 2860 MPa5 mm/min; ASTM D638
Flexural Strength 62.0 MPaISO 178
Flexural Modulus 2420 MPa2 mm/min; ISO 178
 2430 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 36.0 JASTM D256
Izod Impact, Unnotched 367 J/mASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 26.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 5.00 JASTM D3763
Impact Test 1.00 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.23ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.16ASTM D3702 Modified: Manual
K (wear) Factor 8.00 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 99.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
CTE, linear, Transverse to Flow 104 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 147 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 155 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 94.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 195 - 205 °C
Zone 3 210 - 220 °C
Melt Temperature 200 - 215 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80868 / 288815

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.