MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECATEC PPS GW50 PL S0001 natural - plate Polyphenylene Sulfide, Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler

Material Notes: Fillers: glass fibers

Main features:

  • excellent chemical resistance
  • electrically insulating
  • inherent flame resistance
  • very good mechanical strength
Target Industries:
  • automotive industry
  • mechanical engineering
  • oil and gas industry
  • safety engineering
  • sporting goods

Information provided by Ensinger Composites.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.90 g/cc
Filler Content 50.0 %Fiber Volume
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 375 MPaISO 527-4
Tensile Modulus 23.0 GPaISO 527-4
Flexural Strength 500 MPaISO 14125
Flexural Modulus 21.0 GPaISO 14125
Compressive Strength 400 MPaISO 14126
Compressive Modulus 26.0 GPaISO 14126
Shear Strength 88.0 MPainterplanar; ISO 14129
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µm/m-°Cin 0° and 90° direction
Melting Point 285 °C
Maximum Service Temperature, Air 230 °Clong term
 260 °Cshort term
Glass Transition Temp, Tg 90.0 °C
 
Processing PropertiesOriginal ValueComments
Drying Temperature 150 °C
Dry Time 2.00 - 3.00 hour
 
Descriptive Properties
Areal weight finished product312 g/m²
Colornatural
Fiber architecturestyle 7628
Fiber areal weight203 g/m²
Fiber orientation0-90°
Fiber typeE glass
Layers1-95
Material widths625x525 mm
Resin weight content0.349

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN514 / 287738

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.