MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bamberger Polymers Bapolene® 0760 High Density Polyethylene, Blow Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Bapolene® 0760 is a high density polyethylene homopolymer for blow molding applications. It is recommended for applications that require high top load strength and good stiffness. This product meets US FDA 21 CFR 177.1520.

Applications: Blown Containers; Containers; Food Containers; Fruit Juice Bottles.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Food Contact Acceptable; Good Stiffness; Homopolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccASTM D-1505
ESCR 100% Igepal® 8.0 hourASTM D-1693
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 31.1 MPaASTM D-638
Elongation at Break >= 300 %ASTM D-638
Flexural Modulus 1.572 GPaASTM D-638
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
processBlow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
Toyobo Dyneema® SK60 High Strength Polyethylene Fiber
Amco PRIMATOP HDPE 003946HP Blow Molding Polyethylene
Bamberger Polymers Bapolene® 345F Medium Density Polyethylene, Film Extrusion Grade
A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene

PBP3B000 / 20786

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.