MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyLabs U-19 (105) Hydrophobic Energy Absorbing PU Foam
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: U-19 (105) polyurethane exhibits extremely low rebound upon impaction. Density and compression deflection properties can be varied to meet specific requirements. Special hydrophobic formulation eliminates the need for bagging or concerns around sweat or water absorption. Ideally suited for athletic padding, helmet padding and defense impact protection applications.

Properties based on 1/4'' test panels molded at 0.20 g/cm3.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.130 - 0.250 g/cc0.00470 - 0.00903 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 70 - 80
@Time 3.00 sec
70 - 80
@Time 0.000833 hour
Elongation at Break 70 - 95 %70 - 95 %
Tear Strength 0.789 - 1.05 kN/m4.50 - 6.00 pliDie C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYLA962 / 265877

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.