MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Softell CA7469A Thermoplastic Olefinic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Softell CA 7469 A is a reactor TPO (thermoplastic polyolefin) manufactured using the LyondellBasell’ s proprietary Catalloy process technology. It is used for the extrusion and calendaring processes for applications such as TPO skins, W &C and technical compounds. It is also utilized as building block in TPE and TPV compounds. Softell CA 7469 A exhibits low stiffness, low gloss, low hardness and good impact resistance. The grade is available in natural pellet form. Applications: Automotive Parts, Impact Modification, Instrument Panels, Soft Profile & Sheets, TPO Foils and Skins, Wire & Cable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³Method A; ISO 1183-1
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8787ISO 686
Tensile Strength at Break 7.00 MPa1020 psiISO 527-1,-2
Elongation at Break 500 %500 %ISO 527-1,-2
Flexural Modulus 0.130 GPa18.9 ksiISO 178
Charpy Impact, Notched  0.800 J/cm²
@Temperature -40.0 °C
3.81 ft-lb/in²
@Temperature -40.0 °F
ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
 NB
@Temperature -20.0 °C
NB
@Temperature -4.00 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 142 °C288 °FDSC; DSC
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C102 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 50.0 °C122 °FA50; ISO 306
 
Descriptive Properties
Processing MethodCalendaring, Compounding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elastron® V TPV Elastomer
Aurora Plastics TufTech™ 5501124 Vinyl

PEQT8650 / 220284

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.