Notes: Monprene IN-15056 is a general purpose thermoplastic elastomer, available in NAT and pre-colored, designed for the industrial market, including caster wheels. Monprene IN-15056 is a medium hardness, low density, clear grade that exhibits low compression set, good abrasion and chemical resistance, and is suitable for injection molding and extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Abrasion Resistant; Chemical Resistant; Good Colorability; Good Melt Strength; Good Tear Strength; Low Compression Set; Medium Hardness; Low Density; Low Specific Gravity; Weather Resistant Uses: Building Materials; Expansion Joint; Gaskets; Glazing; Hose; Industrial Applications; Outdoor Applications; Pipe Seals; Potable Water Applications; Roof Vents; Rubber Replacement; Strain Reliefs; White Goods & Small Appliance; Windows & Doors RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |