MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ LUX1814N PC (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: 0

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 3.2 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPa50 mm/min; ASTM D638
Elongation at Break 91 %50 mm/min; ASTM D638
Elongation at Yield 7.0 %50 mm/min; ASTM D638
Tensile Modulus 2300 MPa50 mm/min; ASTM D638
Flexural Yield Strength 98.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2370 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 826 J/mASTM D256
 112 J/m
@Temperature -30.0 °C
ASTM D256
Dart Drop, Total Energy 72.0 Jpeak; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 66.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 67.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 141 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 145 °CRate B/50; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Zone 1 165 °CExtrusion
Zone 2 170 °CExtrusion
Zone 3 175 °CExtrusion
Zone 4 180 °CExtrusion
Melt Temperature 180 - 200 °C
Roll Temperature 175 - 180 °CRoll Stack Temperature - Bottom
 175 - 180 °CRoll Stack Temperature - Middle
 175 - 180 °CRoll Stack Temperature - Top
Drying Temperature 75.0 - 90.0 °CExtrusion
Dry Time 2.00 - 4.00 hourExtrusion
Moisture Content >= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10492 / 243959

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.