MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sulfur bearing Copper, UNS C14700, H02 Temper 6 mm and 13 mm rods
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: screw machine products and parts requiring high conductivity, extensive machining, corrosion resistance, copper color, or a combination of these: electrical connectors, motor and switch components, plumbing fittings, cold headed and machined parts, cold forgings, furnace-brazed articles, screws, soldering coppers, rivets and welding torch tips.

Test specimen: rod - 6mm and 13mm diameters.

Key Words: C111, ISO CuSP, CEN CW114C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.94 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 43
Tensile Strength, Ultimate 295 MPa
Tensile Strength, Yield 275 MPa
@Strain 0.5 %
Elongation at Break 18 %
@Diameter 6.00 mm
in 50 mm
 20 %
@Diameter 13.0 mm
in 50 mm
Modulus of Elasticity 115 GPa
Poissons Ratio 0.31Calculated
Machinability 85 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %
Shear Modulus 44.0 GPa
Shear Strength 180 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000181 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 100 °C
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.385 J/g-°C
Thermal Conductivity 374 W/m-K
@Temperature 20.0 °C
Melting Point 1067 - 1076 °C
Solidus 1067 °C
Liquidus 1076 °C
Annealing Point 800 - 1200 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 650 °C
Hot-Working Temperature 750 - 875 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 99.4 - 99.8 %includes Ag
Other, total <= 0.10 %
Sulfur, S 0.20 - 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek Copper Ni Si Cast UNS C81540 High Conductivity
Zirconium Copper (Amzirc Brand Copper), UNS C15000, TH01 Temper
Zirconium Copper (Amzirc Brand Copper), UNS C15000, TH04 Temper
Cadmium-Copper, Deoxidized, UNS C14300 OS025 Temper
Cadmium-Copper, Deoxidized, UNS C14300 H10 Temper

MC14700b4 / 10628

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.