MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Afton Plastics 9302 Fluorinated Ethylene Propylene
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP); Fluorinated Ethylene Propylene (FEP), Molded/Extruded

Material Notes: FEP is a copolymer of tetrafluoroethylene and hexafluoropropylene. This melt processable fluoropolymer exhibits excellent resistance to heat, wear and chemicals.

Product Benefits: • Negligible moisture absorption • Low coefficient of friction • Non-stick surfaces • Chemically inert to most industrial chemicals and solvents • Exceptional dielectric insulation properties • High degree of stress crack resistance • Very low gas permeation and outgassing • Compatible with hot air welding equipment • Temperature range: -400°F to +392°F • High resistance to outdoor weathering.

Typical Application: Pump housings and pipe linings • Fluid handling or chemical processing equipment • Semiconductor wet bench equipment • Hostile environment involving chemical, thermal or mechanical stress • Food processing and packaging equipment • Medical components.

Made from Teflon®, a Chemours product, processed into shapes and components by Afton plastics.

Information provided by Afton Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.12 - 2.17 g/cc2.12 - 2.17 g/ccASTM D792
Water Absorption <= 0.010 %
@Time 86400 sec
<= 0.010 %
@Time 24.0 hour
ASTM D570
Melt Flow 2.0 - 3.9 g/10 min2.0 - 3.9 g/10 minASTM D2216
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55 - 5655 - 56ASTM D2240
Tensile Strength 30.0 MPa4350 psiASTM D638
Elongation at Break 300 - 325 %300 - 325 %ASTM D638
Flexural Modulus 0.655 GPa95.0 ksiASTM D790
Izod Impact, Notched <= NB<= NBASTM D256
Coefficient of Friction 0.250.25ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+18 ohm-cm1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square 1.00e+16 ohm1.00e+16 ohmASTM D257
Dielectric Constant <= 2.15
@Frequency 1000 Hz
<= 2.15
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 78.7 kV/mm
@Thickness 10.0 mm
2000 kV/in
@Thickness 0.394 in
short time; ASTM D149
Dissipation Factor <= 0.00030
@Frequency 1000 Hz
<= 0.00030
@Frequency 1000 Hz
ASTM D150
Arc Resistance >= 180 sec>= 180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 - 260 °C491 - 500 °FASTM D3418
Maximum Service Temperature, Air 205 °C401 °Fcontinuous
Minimum Service Temperature, Air -240 °C-400 °F
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
Solvay A5000 FEP Fluoropolymer
Saint-Gobain Chemfab® 3 Anti-Static PTFE-Coated Glass
Quadrant Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet)
Quadrant Symalit® 1000 PFA unfilled, lining industries (ISO Data)

PAFTON906 / 232131

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.