MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Henkel Loctite® ABLESTIK TE 3530 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: White

Cure: Heat Cure

Product Benefits:

  • One component
  • Thermally conductive
  • Low viscosity
  • Low temperature cure
Application: Assembly

Typical Package Application: Sensor attach and Die attach

LOCTITE ABLESTIK TE 3530 adhesive is designed for bonding heat dissipation components and can be applied by automatic syringe dispense. It cures at moderate to low temperatures allowing it to be used on heat sensitive materials.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.70 g/cc
Viscosity 60000 cP
@Shear Rate 10.0 1/s
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87Cured
Tensile Modulus 180 MPa
@Temperature 200 °C
Cured, Young's
 200 MPa
@Temperature 150 °C
Cured, Young's
 300 MPa
@Temperature 100 °C
Cured, Young's
 1500 MPa
@Temperature 50.0 °C
Cured, Young's
 4700 MPa
@Temperature 25.0 °C
Cured, Young's
 10000 MPa
@Temperature 0.000 °C
Cured, Young's
 16000 MPa
@Temperature -20.0 °C
Cured, Young's
 20000 MPa
@Temperature -40.0 °C
Cured, Young's
Shear Strength >= 8.00 MPaTensile Lap, On Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmCured
Surface Resistance 1.00e+14 ohm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 36.0 µm/m-°CCured
Thermal Conductivity 2.30 W/m-KCured
Glass Transition Temp, Tg 55.0 °CCured, DMA
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
@Temperature 150 °C
 15.0 min
@Temperature 120 °C
 30.0 min
@Temperature 100 °C
Shelf Life 0.100 Month
@Temperature 18.0 - 25.0 °C
3 days
 6.10 Month
@Temperature -25.0 - -18.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT5068 / 255279

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.