MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mateck Magnesium Fluoride (MgF2)
Categories: Ceramic; Halide

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.18 g/cc
Solubility 0.0076 ppm
a Lattice Constant 4.64 Å
c Lattice Constant 3.06 Å
Molecular Weight 62.32 g/mol
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 2890MPa
 4410MPa
Hardness, Mohs 6.0
Modulus of Elasticity 79.7 GPaparallel to c-axis
 169.1 GPaperpendicular to c-axis
Poissons Ratio 0.577
Shear Modulus 57.1 GPaperpendicular to c-axis
 95.2 GPaparallel to c-axis
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.23 - 9.25 µm/m-°C
@Temperature -60.0 - 60.0 °C
perpendicular to c-axis
 10.86 - 14.54 µm/m-°C
@Temperature -60.0 - 60.0 °C
parallel to c-axis
Specific Heat Capacity 0.920 J/g-°C
Melting Point 1255 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.3904at nf'  - nc'
 1.3044
@Wavelength 7000 nm
no
 1.3101
@Wavelength 7000 nm
ne
 1.3618
@Wavelength 3000 nm
no
 1.3724
@Wavelength 3000 nm
ne
 1.3786
@Wavelength 546.1 nm
at ne
 1.4231
@Wavelength 200 nm
no
 1.4367
@Wavelength 200 nm
ne
Transmission, Visible 97 %
@Wavelength 500 nm
Internal Transmittance
IR Transmittance 12 %
@Wavelength 8000 nm
Internal Transmittance
 91 %
@Wavelength 6000 nm
Internal Transmittance
UV Transmittance 95 %
@Wavelength 200 nm
Internal Transmittance
 
Descriptive Properties
Cleavability(100)perfect
 (110)
Constants of Elastic Compliance (Pa^-1)1.053E-11S66
 1.245E-11S11
 -1.66E-12S13
 1.754E-11S44
 5.94E-12S33
 -7.16E-12S12
Symmetrytetragonal
Symmetry Class4/mmm
Thermal Coefficient of Refractive Index1.5E-6 to 1E-6ß0 at 3.39 microns for ±60°C
 1.5E-6 to 1E-6ße at 3.39 microns for ±60°C
Transmission Range (microns)0.13 - 0.7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials AC6043 Titanium Diboride/Boron Nitride Composite
Momentive Performance Materials BIN77 Aluminum Nitride/ Boron Nitride Composite
Silicon Carbide, Reaction-Bonded, SiSiC
M Cubed Technologies HSC-702 Aluminum-toughened Reaction Bonded Silicon Carbide
Envalior TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate

CMAT048 / 87732

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.