MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MRC Polymers NAXALOY™ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled; Polycarbonate (PC)

Material Notes: NAXALOY 770GF16 is a 16% glass filled polycarbonate/ABS blend. This material is available in black, natural and custom colors. It’s typically used for automotive interior applications.

Information provided by MRC Polymers Inc.

Key Words: ABS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Filler Content 16 %ASTM D785
Melt Flow 3.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
nominal; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 97.0 MPaASTM D638
Flexural Strength 21.5 ksiASTM D790
Flexural Modulus 690 ksiASTM D790
Izod Impact, Notched 2.00 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 264 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MRC Polymers NAXALOY™ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled
Daicel CEVIAN® S1210 PC/ABS alloy
Daicel CEVIAN® S1220 PC/ABS alloy
Lotte Advanced Materials Infino® WP-1200 PC/ABS/GF
Covestro Bayblend® T88-4N Polycarbonate + ABS, 20% Glass Filled

PMRC019 / 89448

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.