MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Wacker Wacker® TES 40 WN Silicate
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: WACKER® TES 40 WN is an ethyl silicate providing approximately 41% silicon dioxide (silica) upon complete hydrolysis.

Properties: WACKER® TES 40 WN contains many hydrolysable ethoxy groups. For applications in which the inorganic SiO2 is to be used as a binder, WACKER® TES 40 WN needs to be activated.

Special features:

  • storage-stable, low-viscous binder with a high silica content (41% SiO2, fully hydrolyzed)
  • liquid source of silica with a high flash point
Application: WACKER® TES 40 WN is used for the precipitation of silica upon complete hydrolysis. The SiO2 coating firmly binds inorganic fillers and pigments and adheres well to different inorganic substrates like glass, ceramics or metall. Chemical and mechanical properties of the substrates can be improved by the thin SiO2 film, which is also highly heat-resistant.
  • binder for zinc-rich anti-corrosion paints
  • binder for refractory fillers (production of ceramic shells and cores)
  • precision casting
  • coating material for pigments and fibers
  • liquid source of SiO2 as a (film-forming) binder
  • crosslinking agent, e.g. for silicone elastomers
  • sol-gel processes

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 - 1.07 g/cc0.0383 - 0.0387 lb/in³DIN 51757
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 10<= 10[mg/kg]
 
Thermal PropertiesMetricEnglishComments
Flash Point 62.0 °C144 °FDIN 51755
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Clear" but manufacturer does not quantify.
 
Component Elements PropertiesMetricEnglishComments
SiO2 41 %41 %
 
Descriptive Properties
Appearancecolorless, clear
Color<10 APHA
Content<10 mg/kgHydrolyzable chloride

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Laponite® S485 Magnesium Aluminum Silicate
Imerys Hydrated Aluminum Silicate KT 90A-1 Kaolin
Evonik ULTRASIL® AS 7 Sodium/Aluminum Silicate
Du-Co Ceramics DC-142 Aluminum Silicate
Corning Pyroceram® Code 9606 Glass Ceramic

PWACK9822 / 205351

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.