MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Pluracol® 4156 Slabstock Foam Polyol
Categories: Fluid

Material Notes: Description: Pluracol® 4156 polyol is a 56 hydroxyl number (nominal 3000 molecular weight) polyether triol capable of producing a broad range of flexible slabstock polyurethane foams for furniture, bedding and carpet underlay applications. This polyol has been formulated with a low volatile inhibitor package designed for either conventional curing or mechanical forced air curing. Pluracol 4156 provides a consistent processing profile on trough and fallplate machines.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/cc
@Temperature 45.0 °C
 1.01 g/cc
@Temperature 35.0 °C
 1.02 g/cc
@Temperature 25.0 °C
Viscosity 210 cP
@Temperature 45.0 °C
 355 cP
@Temperature 35.0 °C
 582 cP
@Temperature 25.0 °C
Molecular Weight 3000 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.010STI 3063/3161
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.16 J/g-°C
Thermal Conductivity 0.125 W/m-K
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %STI 3062
 
Descriptive Properties
ColorClear Liquid
Hydroxyl Number54.5 - 57.5 mg KOH/gSTI 3007/3162

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 2-8692 Fluid
BASF Pluracol® SG-470 Rigid Polyol

PBASG0788 / 132421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.