MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Osprey 18Ni300 Tool Steel Powder
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Tool Steel

Material Notes: Particles produced by gas atomization are spherical and can be produced in various sizes to accommodate various processing/printing techniques such as metal injection molding (MIM), additive manufacturing, plasma/thermal spray, or hot isostatic pressing (HIP).

Information provided by Sandvik Osprey.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.10 %
Carbon, C <= 0.030 %
Chromium, Cr <= 0.30 %
Cobalt, Co 9.0 %
Iron, Fe 67 %As Balance
Manganese, Mn <= 0.10 %
Molybdenum, Mo 4.8 %
Nickel, Ni 18 %
Silicon, Si <= 0.10 %
Titanium, Ti 0.70 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Osprey A6 Tool Steel Powder
Crucible Steel CPM® S110V® Stainless Tool Steel
Sandvik Osprey 1.2709 Tool Steel Powder
Bohler-Uddeholm BÖHLER S692/S693 MICROCLEAN® PM M4 High Speed Steel
Crucible Compaction Metals P/M 625 Corrosion Resistant Alloy

NSANDV9915 / 220763

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.