MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SACO AEI PEXIDAN® HF V/T Moisture-curable Low Smoke Zero-Halogen (LSZH)
Categories: Polymer; Thermoplastic

Material Notes: Solar UV resistant, silane crosslinkable, Halogen Free, flame retardant compound for low-voltage building wire applications (VW-1 Rated – styles XHHW-2, RHW-2, RHH, and SIS)

PEXIDAN® HF V/T is a unique low smoke halogen-free flame retardant 90°C wet-rated XL-insulation system curable by moisture. It consists of a silane pre-grafted base compound SX653 and a catalyst masterbatch CM540U. Mixed and extruded in the proper proportions (95:5), the two components result in a material that is cross-linkable by exposure to 90°C hot water. PEXIDAN® HF V/T is REACH and RoHS-compliant. Wire made with PEXIDAN® HF V/T may be marked VW-1, as well as Oil Resistant “PR I” and “PR II”, Gas & Oil Resistant “GR I” and “GR II”, “-40C” and “SUNRES” in all colors.

Information provided by SACO AEI Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.64 g/ccASTM D792
Deformation 3.0 %UL 1581 / UL 2556
Storage Temperature <= 30.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2090 psiUL 1581 / UL 2556
 1690 psi
@Treatment Temp. 100 °C,
Time 346000 sec
After 96 hours oil; UL 1581 / UL 2556
 1900 psi
@Treatment Temp. 100 °C,
Time 5.18e+6 sec
After 60 day oil; UL 1581 / UL 2556
 2400 psi
@Treatment Temp. 121 °C,
Time 605000 sec
after thermal ageing; UL 1581 / UL 2556
Elongation at Break 167 %UL 1581 / UL 2556
 132 %
@Treatment Temp. 100 °C,
Time 346000 sec
After 96 hours oil; UL 1581 / UL 2556
 149 %
@Treatment Temp. 121 °C,
Time 605000 sec
after thermal ageing; UL 1581 / UL 2556
 150 %
@Treatment Temp. 100 °C,
Time 5.18e+6 sec
After 60 day oil; UL 1581 / UL 2556
Tensile Set 2.5 %
@Treatment Temp. 150 °C,
Time 900 sec
Hot set after 41% elongation under load, 20N/cm2; SACO AEI DWI-QA-4007 based on ICEA T-28-562
Crush Resistance 1857 lb (mass)UL 1581 / UL 2556
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.76
@Frequency 60 Hz,
Temperature 90.0 °C
(SIC); UL 1581 / UL 2556
Dielectric Breakdown 15540 Vafter glancing impact; UL 1581 / UL 2556
 42000 Vinitial; UL 1581 / UL 2556
 
Thermal PropertiesOriginal ValueComments
Smoke Density 139.3Non-flaming, Dsmax (corrected); ASTM E662
 176.6Flaming, Dsmax (corrected); ASTM E662
 29.7
@Time 240 sec
Flaming, Ds; ASTM E662
 30.8
@Time 240 sec
Non-flaming, Ds; ASTM E662
Oxygen Index 38 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 154 - 171 °Cbarrel zones
Die Temperature 179 °C
Head Temperature 177 °C
 
Descriptive Properties
Degree of Cross-linking86%ASTM D2765
Flame ResistancePasses FT2UL 1581; UL 2556
 Passes VW-1UL 1581; UL 2556

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO071 / 265501

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.