Product Description: 3M™ Dyneon™ FPO 3730 is a peroxide curable fluoroelastomer terpolymer containing 69.8 wt% fluorine. FPO 3730 can be used in compression, transfer or injection molding, and extrusion processes. Features and Benefits: - Good processability
- Excellent physicals
- Broad chemical resistance
Information provided by 3M™ |