MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ 797 Cyanoacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Chem-Set 797 is a cyanoacrylate adhesive with good impact strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and has very good gap filling capabilities. The product adheres to a variety of surfaces including steel, aluminum, galvanized steel, plastics, and elastomers.

Features & Benefits: Longer cure allows accurate alignment, Ease of use – no mixing or heat cure, Bonds most materials, 100% reactive, no solvents.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccuncured
Viscosity 3000 - 5000 cP
@Temperature 25.0 °C
uncured
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 2900 - 3625 psisteel;; ASTM D1002
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 10.0 V/milcured
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°Ccured
Thermal Conductivity 0.100 W/m-Kcured
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 - 10.0 seccured, steel
 8.00 - 12.0 seccured, Buna N Rubber
 24.0 hourFull
Shelf Life 6.00 MonthIn original unopened containers.
 
Descriptive Properties
Chemical CompositionEthyl Cyanoacrylate
Chemical Resistance100% retention Isopropanol, 1000 hrs @ 22°C
 100% retention, Air Reference for 1000 hrs @22°C
 110% retention, Ethanol, 1000 hrs @ 22°C
 110% retention, Motor oil, 1000 hrs @ 40°C
 55% retention, 1000 hrs @ 22°C
 55% retention, 95% RH @ 40°C
 85% retention, Unleaded gasoline, 1000 hrs @ 22°C
Colorcolorless
Gap FillingMax. 0.020 inches, cured
Temperature Resistance100% retention @ -25°C
 100% retention @ 40°C
 19% retention @ 150°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEMI930 / 232183

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.