MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced, Impact Modified

Material Notes: Description

Polyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Melt Flow 8.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2600 psiat max load, 2 in/min; ASTM D638
Elongation at Break 20 %ASTM D638
Flexural Strength 3500 psiASTM D790
Flexural Modulus 222000 psitangent; ASTM D790
Flexural Modulus, 1% Secant 195000 psiASTM D790
Izod Impact, Notched 5.00 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYFORT™ FPP 3063UV-3120 Black, UV Stabilized Modified Polypropylene
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene
A. Schulman POLYFORT™ FPP 3459 Glass Filled Impact Copolymer
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene
A. Schulman POLYFORT™ FPP 1237 CaCO3 filled homopolymer polypropylene

PASHU160 / 25124

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.