MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 1235-O Foil
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 1000 Series Aluminum

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
The aluminum content for unalloyed aluminum not made by a refining process is the difference between 100.00 percent and the sum of all other analyzed metallic elements present in amounts of 0.010 percent of more each, expressed to the second decimal before determining the sum. For alloys and unalloyed aluminum not made by a refining process, when the specified maximum limit is 0.XX, an observed value or a calculated value greater than 0.005 but less than 0.010% is rounded off and shown as " less than 0.01%".
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 1235-O Foil; AA1235-O Foil; UNS A91235; Al1235-O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.705 g/cc0.09772 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 4545500 kg load with 10 mm ball. Calculated value.
Tensile Strength, Ultimate 75.0 MPa10900 psi
Tensile Strength, Yield 30.0 MPa4350 psi
Elongation at Break 2.4 %2.4 %Foil
Tensile Modulus 69.0 GPa10000 ksiCompressive modulus in is typically about 2% higher for Al alloys
Poissons Ratio 0.330.33Estimated from trends in similar Al alloys.
Shear Modulus 26.0 GPa3770 ksiEstimated from similar Al alloys.
Shear Strength 100 MPa14500 psiCalculated value.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000280 ohm-cm0.00000280 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 390 J/g168 BTU/lb
CTE, linear  23.6 µm/m-°C
@Temperature 20.0 - 100 °C
13.1 µin/in-°F
@Temperature 68.0 - 212 °F
 25.5 µm/m-°C
@Temperature 20.0 - 300 °C
14.2 µin/in-°F
@Temperature 68.0 - 572 °F
average
Specific Heat Capacity 0.900 J/g-°C0.215 BTU/lb-°F
Thermal Conductivity 230 W/m-K1600 BTU-in/hr-ft²-°F
Melting Point 645 - 655 °C1190 - 1210 °F
Solidus 645 °C1190 °F
Liquidus 655 °C1210 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al >= 99.35 %>= 99.35 %Specified
Copper, Cu <= 0.05 %<= 0.05 %
Magnesium, Mg <= 0.05 %<= 0.05 %
Manganese, Mn <= 0.05 %<= 0.05 %
Other, each <= 0.03 %<= 0.03 %
Si+Fe <= 0.65 %<= 0.65 %
Titanium, Ti <= 0.06 %<= 0.06 %
Vanadium, V <= 0.05 %<= 0.05 %
Zinc, Zn <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 1235-H19 Foil
Aluminum 1145-O
Aluminum 1100-O
8079 Aluminum Composition Spec
Aluminum 1050-O

MA1235O / 8793

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.