MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Monprene® WR-12232 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene WR-12231 is a specialty high performance thermoplastic elastomer designed for a variety of consumer application, including writing instrument grips requiring a soft, rubber-like feel. Monprene WR-12231 is a lubricated, low medium hardness, low density grade containing an antimicrobial additive. This grade is suitable for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive:Antimicrobial (Fungicide)

Features: Bacteria Resistant; Fungus Resistant; Medium Flow; Low Density; Low Hardness; Low Specific Gravity; Lubricated; Slip; Without Fillers

Uses: Consumer Applications; Flexible Grips; Handles; Sporting Goods; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ASTM D792
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 200 °C
15 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  32
@Time 5.00 sec
32
@Time 0.00139 hour
Injection Molded; ASTM D2240
 35
@Time 1.00 sec
35
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 2.55 MPa370 psiDie C, 20 in/min, Flow; ASTM D412
 7.17 MPa1040 psiDie C, 20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain  0.317 MPa
@Strain 100 %
46.0 psi
@Strain 100 %
Die C, 20 in/min, Across Flow; ASTM D412
 0.614 MPa
@Strain 300 %
89.0 psi
@Strain 300 %
Die C, 20 in/min, Across Flow; ASTM D412
 0.869 MPa
@Strain 100 %
126 psi
@Strain 100 %
Die C, 20 in/min, Flow; ASTM D412
 1.34 MPa
@Strain 300 %
195 psi
@Strain 300 %
Die C, 20 in/min, Flow; ASTM D412
Elongation at Break 690 %690 %Die C, 20 in/min, Flow; ASTM D412
 2000 %2000 %Die C, 20 in/min, Across Flow; ASTM D412
Tear Strength 13.8 kN/m79.0 pliDie C, 20 in/min, Flow; ASTM D624
 16.8 kN/m96.0 pliDie C, 20 in/min, Across Flow; ASTM D624
Compression Set  14 %
@Temperature 22.8 °C,
Time 79200 sec
14 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 44 %
@Temperature 70.0 °C,
Time 79200 sec
44 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 199 - 249 °C390 - 480 °FMelt, Injection
Rear Barrel Temperature 182 - 232 °C360 - 450 °FInjection
Middle Barrel Temperature 188 - 238 °C370 - 460 °FInjection
Front Barrel Temperature 193 - 243 °C380 - 470 °FInjection
Nozzle Temperature 199 - 249 °C390 - 480 °FInjection
Zone 1 182 - 232 °C360 - 450 °FExtrusion
Zone 2 188 - 238 °C370 - 460 °FExtrusion
Zone 3 193 - 243 °C380 - 470 °FExtrusion
Zone 4 199 - 249 °C390 - 480 °FExtrusion
Zone 5 199 - 249 °C390 - 480 °FExtrusion
Die Temperature 199 - 249 °C390 - 480 °FExtrusion
Mold Temperature 35.0 - 48.9 °C95.0 - 120 °FInjection
Injection Pressure 1.38 - 5.52 MPa200 - 800 psiInjection
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0968 / 237459

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.