MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polykemi AB POLYfill PPH T16020 Polypropylene Homopolymer, Mineral Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes:

Information provided by Polykemi AB

Key Words: Polypropylene Homopolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Filler Content 20 %±2%; Polykemi
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cmISO 2577
Melt Index of Compound 16 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break <= 34.0 MPaISO/R527
Elongation at Break 25 %ISO/R527
Elongation at Yield 6.0 %ISO/R527
Flexural Strength <= 51.0 MPaISO 178
Flexural Modulus 2800 MPa
@Temperature 23.0 °C
ISO 178
Charpy Impact Unnotched 18.0 kJ/m²
@Temperature -20.0 °C
ISO 179
 35.0 kJ/m²
@Temperature 23.0 °C
ISO 179
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -20.0 °C
ISO 179
 3.00 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 - 80.0 µm/m-°CPolykemi
Deflection Temperature at 0.46 MPa (66 psi) 118 °C120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C120°C/h; ISO 75/1
Vicat Softening Point 86.0 °C
@Load 5.001 kg
50°C/h; ISO 306
 148 °C
@Load 1.00 kg
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
Glow Wire Test 750 °C
@Thickness 2.00 mm
IEC 695-2-1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 205 - 260 °C
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 70.0 - 80.0 °C
Dry Time 2 - 4 hourin circulation dryer
 2 - 4 hourin desiccant air dryer
Injection Pressure 40.0 - 110 MPa
Back Pressure 1.00 - 2.00 MPa
 
Descriptive Properties
Holding Pressure20-40% of injection pressure
Injection SpeedHigh
Scratch Resistance, 10N (dL)3.310N Fine Structure; ISO 1518/D65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom ZB 752 AC T 2065 (EBONY) Polypropylene, Talc Filled
LyondellBasell Hostacom X M3 N07 105555 Polypropylene with 30% Talc Filler
LyondellBasell Hostacom Hostacom HYP 376D NAT Polypropylene, Mineral Reinforced
LyondellBasell Hostacom 1103 NATURAL Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 2-2120 20% Talc-Filled Polypropylene Block-Copolymer

PPOLYK384 / 123109

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.