MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Greene Tweed AR™ 1 Abrasive-Resistant Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: Sand and other abrasives are often a challenge for pump users in the power industry. Clearances on line shaft bearings and bowl wear rings open up, increasing pump vibrations and reducing pump efficiency. Greene Tweed’s proprietary AR™ thermoplastic materials exhibit outstanding wear characteristics in media containing solids.

AR1 offers excellent abrasive resistance as well as chemical resistance approaching that of PTFE. AR1 is rated from ambient to 120°F (49°C). AR1 is easy to machine, and clearance requirements are easily determined. AR1 works well in a variety of pumps in the power industry including those working with circulating water as well as screen wash pumps. AR materials have performance characteristics that exceed traditional technologies such as cutlass rubber, bronze and carbon materials.

Applications:

  • Circulating water pumps
  • Open and closed cooling water pumps
  • River water pumps
  • Screen wash pumps
  • Sump pumps

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.00 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength, Yield 2270 psiASTM D4745
Elongation at Break 300 %ASTM D1457
Tensile Modulus 165000 psiASTM D638
Flexural Strength 2790 psiat 5% strain; ASTM D790
Flexural Modulus 157000 psiASTM D790
Compressive Strength 2700 psiASTM D695
Compressive Modulus 139000 psiASTM D695
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µin/in-°F
@Temperature 100 °C
Maximum Service Temperature, Air 120 °F
Minimum Service Temperature, Air 60.0 °F
 
Descriptive Properties
ColorBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Nilit Nilamid A3 H G8 40% Glass Reinforced PA66
G-11 Fiberglass Epoxy Laminate Sheet
G-10 Fiberglass Epoxy Laminate Sheet
Greene Tweed Avalon® 56 PTFE
Greene Tweed Avalon® 57 PTFE, Thermoset Resin Filled

PGREEN69 / 42363

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.