Taro Plast Tarolox 10 G4 X0 PBT, 20% Glass Fiber Reinforced, Flame Retardant
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
Material Notes:
PBT medium viscosity, 20% glass fibers reinforced, flame retardant UL94 V0. Available: all colors, heat stabilized (H), UV stabilized (L), release agent (W).
Information provided by Taro Plast S.p.a.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.57
-
1.59
g/cc
0.0567
-
0.0574
lb/in³
ISO 1183
Filler Content
20 %
20 %
ISO 3451
Water Absorption
0.050 %
@Time 86400 sec
0.050 %
@Time 24.0 hour
ISO 62
Water Absorption at Saturation
0.25 %
0.25 %
ISO 62
Linear Mold Shrinkage, Flow
0.0040
-
0.0060
cm/cm
0.0040
-
0.0060
in/in
ISO 2577
Linear Mold Shrinkage, Transverse
0.0060
-
0.0090
cm/cm
0.0060
-
0.0090
in/in
ISO 2577
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
110
MPa
16000
psi
ISO 527
Elongation at Break
3.0 %
3.0 %
ISO 527
Tensile Modulus
8.00
GPa
1160
ksi
ISO 527
Flexural Strength
165
MPa
23900
psi
ISO 178
Flexural Modulus
7.50
GPa
1090
ksi
ISO 178
Izod Impact, Notched
0.650
J/cm
1.22
ft-lb/in
127x12.7x3.2; ASTM D256
Charpy Impact, Notched
0.550
J/cm²
2.62
ft-lb/in²
80x10x4; ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
>=
1.00e+15
ohm-cm
ASTM D257
Comparative Tracking Index
175
V
175
V
(M), Method B; IEC 60112
250
V
250
V
Method A; IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear
30.0
µm/m-°C
16.7
µin/in-°F
ISO 11359
Maximum Service Temperature, Air
90.0
°C
@Time 468000 sec
194
°F
@Time 130 hour
IEC 60216
Hot Ball Pressure Test
215
°C
419
°F
IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
215
°C
419
°F
ISO 75/A
Deflection Temperature at 1.8 MPa (264 psi)
205
°C
401
°F
ISO 75/A
Vicat Softening Point
210
°C
@Load 5.00 kg
410
°F
@Load 11.0 lb
ISO 306
215
°C
@Load 1.00 kg
419
°F
@Load 2.20 lb
ISO 306
Flammability, UL94
V-0
@Thickness 0.970 mm
V-0
@Thickness 0.0382 in
127x2.17xThickness
Oxygen Index
31 %
31 %
6.3x12.7x3.2; ASTM D2863
Glow Wire Flammability Index
960
°C
@Thickness 2.00 mm
1760
°F
@Thickness 0.0787 in
60x60xThickness; IEC 60695-2-12
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PTARO082 / 283190
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.