MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® H70E-4 Thermally Conductive Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Product Description: EPO-TEK® H70E-4 is a two component, thermally conductive, electrically insulating epoxy adhesive for semiconductor, microelectronic and opto-electronic packaging. It may be used for heat sinking power devices in the form of hybrid circuits or at the SMD / PCB level.

Advantages & Application Notes:

  • Thixotropic epoxy which is paste-like and non-flowing. It has adhesive strength before cure.
  • Paste-like rheology allows it to be applied by automated dispensing or screen printing techniques. Other methods, including by tooth-pick, are acceptable.
  • Suggested Applications:
    • PCB:
      • Bonding heat sinks; Adhesion to Al, Cu, most metals and plastics
      • Bonding SMDs to PCB; Adhesion to FR4, flex PCB, active and passive SMT packages; staking SMDs to PCB for double sided circuits
      • Bonding ferrites and magnets for electronic sub-assemblies
    • Semiconductor: die attach onto substrates; COB and direct-chip attach
    • Hybrid: bonding heat sinks and substrate attach to metal case
    • Opto-electronic: active alignment of optics and fiber optic components
  • User friendly 1:1 mix ratio allows for static mixing, or specialty packaging, with lengthy pot-life available.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.61 g/ccPart A
 2.02 g/ccPart B
Particle Size <= 20 µm
Viscosity 20000 - 40000 cP
@Temperature 23.0 °C
20 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67
Tensile Modulus 417000 psiStorage
Shear Strength 1070 psiLap
 >= 1700 psiDie
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 2.50e+13 ohm-cm
Dielectric Constant 4.81
@Frequency 1000 Hz
Dissipation Factor 0.0179
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°CBelow Tg
 77.0 µm/m-°CAbove Tg
Thermal Conductivity 0.570 W/m-K
Maximum Service Temperature, Air 200 °CContinuous
 300 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 80.0 °CDynamic Cure 20200°C /ISO 25 Min; Ramp -40200°C @ 20°C/Min
Decomposition Temperature 432 °CDegradation Temperature
 
Processing PropertiesOriginal ValueComments
Cure Time 12.0 hour
@Temperature 50.0 °C
Minimum Bond Line
 15.0 min
@Temperature 120 °C
Minimum Bond Line
Pot Life 3600 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Descriptive Properties
ColorDark GrayPart A
 Dark GrayPart B
ConsistencySmooth thixotropic paste
Mix Ratio by Weight1:1
Number of ComponentsTwo
Thixotropic Index3.2
Weight Loss0.57%200°C
 1.49%250°C
 3.09%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H61 Thermally Conductive Epoxy
Epoxy Technology EPO-TEK® H63 Thermally Conductive, Electrically Insulating Epoxy
Atom Adhesives AA-DUCT 905 Epoxy Adhesive
Epoxy Technology EPO-TEK® H62 Thermally Conductive Epoxy
Epoxy Technology EPO-TEK® H67-MP Thermally Conductive Epoxy

PPOXYT076 / 141115

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.