MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type T2 Tungsten High Speed Tool Steel (UNS T12002)
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Used in high speed tool and cutting applications such as drills, milling processes, reamers, etc. Tungsten content promotes high temperature hardness and wear resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.67 g/cc0.313 lb/in³
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.80 - 0.90 %0.80 - 0.90 %
Chromium, Cr 3.75 - 4.5 %3.75 - 4.5 %
Copper, Cu <= 0.25 %<= 0.25 %
Iron, Fe 70.8 - 75.8 %70.8 - 75.8 %As Balance
Manganese, Mn 0.20 - 0.40 %0.20 - 0.40 %
Molybdenum, Mo <= 1.0 %<= 1.0 %
Nickel, Ni <= 0.30 %<= 0.30 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.20 - 0.40 %0.20 - 0.40 %
Sulfur, S <= 0.030 %<= 0.030 %0.06 to 0.15% may be specified to improve machinability
Tungsten, W 17.5 - 19 %17.5 - 19 %
Vanadium, V 1.8 - 2.4 %1.8 - 2.4 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type T1 Tungsten-Alloy High-Speed-Tool Steel (UNS T12001)
AISI Type T15 Tungsten High Speed Tool Steel (UNS T12015)
AISI Type O6 Tool Steel
AISI Type O1 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 425°C
AISI Type S1 Tool Steel, quenched 955°C (1750°F), tempered 150°C (300°F)

MSTT2 / 172279

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.