MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Molding M5005 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D792
Spiral Flow 58.4 cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 46.2 MPa51 mm/min; ASTM D638
Elongation at Break 29 %51 mm/min; ASTM D638
Tensile Modulus 2740 MPa51 mm/min; ASTM D638
Flexural Strength 73.8 MPaASTM D790
Flexural Modulus 2680 MPaASTM D790
Izod Impact, Notched 110 J/m
@Thickness 3.18 mm,
Temperature -18.0 °C
Injection Molded; ASTM D256A
 160 J/m
@Thickness 3.18 mm,
Temperature 0.000 °C
ASTM D256
 530 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 67.7 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 68.4 °C
@Thickness 3.18 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.3 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 71.9 °C
@Thickness 3.18 mm
Annealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 210 °C
 
Descriptive Properties
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesConstruction Applications
 General Purpose
 Outdoor Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Axiall 1601 Clear 7002 Flexible PVC
Axiall 8150 Rigid PVC, Extrusion & Molding
Colorite Polymers 2007 Rigid PVC
Colorite Polymers 2019F Rigid PVC
Novatec Novablend® 4545 PVC

PH0POL0941 / 145510

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.